Stochastic modelling of chloride-induced pitting corrosion of reinforcement bars in concrete.

L. Llano, Marios Chryssanthopoulos, M. Imran Rafiq, A. Zanker

Research output: Chapter in Book/Conference proceeding with ISSN or ISBNConference contribution with ISSN or ISBNpeer-review